Stainless steel VCR is a commonly used equipment for transporting high-purity chemicals and gases, and its blockage problem has always plagued users. This article will analyze the causes of blockage in stainless steel VCR and propose corresponding solutions.
Reason 1: Accumulation of particle impurities
Stainless steel VCR often encounters blockage by particle impurities during use. These particulate impurities may be metal chips, dust, or other solid particles from the production process. During long-term use, these particles will continuously deposit on the inner wall of the pipeline with the fluid, gradually forming blockages
To address this issue, on one hand, regular cleaning of pipelines can be used to prevent the accumulation of particle impurities. On the other hand, when designing and producing stainless steel VCRs, filters and other devices should be considered to prevent particle impurities from entering the pipeline and avoid blockage
Reason 2: Abnormal moisture content
Stainless steel VCR can transport various chemicals and gases, some of which may contain high levels of moisture. When the moisture content in the liquid exceeds the proportion, it can cause condensation inside the stainless steel VCR, leading to pipeline blockage
To solve this problem, it is necessary to first check whether the moisture content of the conveyed liquid is within the normal range and take dehumidification measures accordingly. Choosing appropriate materials and processing techniques can also reduce the possibility of condensation, thereby reducing the risk of blockage
Reason Three: Abnormal Stress
The pressure that stainless steel VCR needs to withstand during operation. If excessive pressure continues to act inside the pipeline, it can cause deformation or even rupture of the pipe wall, leading to blockage. On the other hand, excessively low pressure may prevent fluid from passing through the pipeline smoothly
To avoid blockage caused by abnormal pressure, users should choose the appropriate pressure range according to their actual situation and regularly check and adjust it. Reasonable design of pipeline systems and selection of appropriate pipeline materials are also important factors in ensuring pressure stability.
The main reasons for the blockage of stainless steel VCR include the accumulation of particle impurities, abnormal water content, and abnormal pressure. To solve these problems, users can take a series of preventive and maintenance measures, such as cleaning pipelines, filtering particle impurities, dehumidification measures, and reasonable pressure management. By using and maintaining it correctly, stainless steel VCR can effectively perform its conveying function and improve the efficiency of chemical and gas transportation